SA662GRC carbon steel plate for medium and low temperature pressure vessels
SA662GRC steel plate corresponding to the GB: 16MNDR European standard: P355NL1
SA662GRC implementation standards: ASTM, ASME standards
ASTM: American Mechanical Association ASME: American Materials Association
National standard: 16MNDR implementation standard: GB/T3531
European standard: P355NL1 implementation standard: EN10025
Heat treatment condition of SA662GRC steel plate: normalizing
Normalizing: The steel plate is heated to an appropriate temperature for cooling in the air
SA662GRC steel plate flaw detection: also known as ultrasonic inspection, is a method of inspection for the internal quality of the steel plate, but also can test the metal internal defects such as (concealed cracks, pores, trachoma and impurities)
SA662GrC中低溫壓力容器用碳鋼板
SA662GrC鋼板對(duì)應(yīng)國(guó)標(biāo):16MnDR 歐標(biāo):P355NL1
SA662GrC執(zhí)行標(biāo)準(zhǔn):ASTM、ASME標(biāo)準(zhǔn)
ASTM:美國(guó)機(jī)械協(xié)會(huì) ASME:美國(guó)材料協(xié)會(huì)
國(guó)標(biāo):16MnDR執(zhí)行標(biāo)準(zhǔn):GB/T3531
歐標(biāo):P355NL1執(zhí)行標(biāo)準(zhǔn) :EN10025
SA662GrC鋼板熱處理狀態(tài):正火
正火:將鋼板加熱到適應(yīng)溫度在空氣中進(jìn)行冷卻
SA662GrC鋼板可進(jìn)行探傷:也被稱為超聲波檢驗(yàn),是針對(duì)鋼板內(nèi)部質(zhì)量的一種檢驗(yàn)方法手段,同時(shí)也可以檢驗(yàn)出金屬內(nèi)部的缺陷如(隱蔽裂紋、氣孔、沙眼和雜質(zhì)等)
SA662GrC鋼板化學(xué)成分(Wt%)
牌號(hào)
化學(xué)成分(熔煉分析)%
C:碳
Si:硅
Mn:錳
P:磷
S:硫
ALs:酸熔鋁
SA622GrC
≤0.20
0.15-0.50
1.0-1.6
≤0.035
≤0.04
≥0.020
舞鋼可提供的熱處理(正火、回火、淬火、退火等):
正火:將鋼板加熱到適當(dāng)溫度在空氣中進(jìn)行冷卻
回火:將鋼板在某一適當(dāng)溫度下進(jìn)行長(zhǎng)時(shí)間保溫在冷卻
淬火:將鋼板加熱保溫后在水油或其他無(wú)機(jī)鹽等介質(zhì)中進(jìn)行快速冷卻
退火:將鋼板加熱到適宜溫度根據(jù)材料和規(guī)格的不同進(jìn)行緩慢冷卻